In the PDP test, the voltage is scanned from a low potential to a high potential. Therefore, usually, reaction (5) occurs at the working electrode/electrolyte interface from the beginning, which may result in the generation of a large amount of hydroxide ions and promote the precipitation of Mg(OH)2 at the corrosion site.