In Figure 4, it was found that the tensile specimen broke suddenly near the yield point, especially for larger PAG and higher H2 pressure. Therefore, it seems meaningless to discuss the PUE of these specimens.
In Figure 4, it is found that the stretch sample breaks suddenly near the yield point, especially for larger PAGs and higher H2 pressures. Therefore, there seems to be no point in discussing the PUEs of these specimens.
In Figure 4, it is found that the tensile specimen breaks suddenly near the yield point, especially for larger PAG and higher H2 pressure. Therefore, it seems meaningless to discuss the pue of these specimens.<br>